Material Notes:
Key Features: fractional melt flow, medium modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convoluted tubingDescription: Hifax ETA-5081 fractional melt flow, blow molding grade thermoplastic olefin resin combines good processability with balanced strenght, thoughness and flexibility. It was deisgne for various automotive under-the-hood applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
Tool, Montell
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 0.480 GPa
69.6 ksi
Tangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256A
Gardner Impact 29.0 J

@Temperature -30.0 °C
21.4 ft-lb

@Temperature -22.0 °F
ASTM D3029
Impact Test 26.0 J

@Temperature -30.0 °C
19.2 ft-lb

@Temperature -22.0 °F
Dynatup Impact, E at Max Load, Ductile; ASTM D3763
Tear Strength 110 kN/m
628 pli
ASTM D624
Users viewing this material also viewed the following: