Lubriplate Temp G.S. Low Lithium Based Grease For Open Gearing

Category Fluid , Lubricant , Lithium Gellant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate Temp G.S. Low Lithium Based Grease For Open Gearing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Applications: Open gears, slides, fifth wheels, low temps. Gear Shield Series Greases are available in Cans, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 300 SUS
300 SUS
Kinematic Viscosity at 40°C (104°F) 58 cSt
58 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 265
265
Unknown Amount of Work
Penetration P(60), 1/10 mm 295
295
Unknown Amount of Work
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Approx. Cold test
Dropping Point 204 °C
400 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW
NLGI Grade 2
Rust/Oxidative Additives YES
Water Resistant YES