Lubriplate Food Grade Cooker Oil USP Mineral -Based Food Machinery Grade

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate Food Grade Cooker Oil USP Mineral -Based Food Machinery Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This zinc free oil is designed for use in the Manzel Lubricators and Micro-valve systems found on most cookers and sterilizers used in canning operations and other similar applications involving high temperature and high humidity conditions. Unique additives provide high load-carrying ability and corrosion protection.Available in Bottles, Jugs, Pails, 1/4 Drums and DrumsH-1 Class Lubricants are manufactured with ingredients that comply with FDA regulation 21 CFR 178.3570 for lubricants with incidental contact with the edible product.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 104
104
Viscosity Index
150
150
ISO Grade
Saybolt Viscosity at 100°F 795 SUS
795 SUS
Saybolt Viscosity at 210°F 82 SUS
82 SUS
Kinematic Viscosity at 40°C (104°F) 155 cSt
155 cSt
Kinematic Viscosity at 100°C (212°F) 16 cSt
16 cSt
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
Flammability Test 525
525
[°F] Fire Point
Flash Point 246 °C
475 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 90
SAE No. 40