Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubriplate 78 Cooker Oil Food Machinery Oil

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate 78 Cooker Oil Food Machinery Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Class H-2** oil, for use in Manzel lubricators for A-B cookers and sterilizers, FMC cookers. Corrosion and oxidation resistant.Available in Bottles, Jugs, Pails, 1/4 Drums and DrumsH-1 Class Lubricants are manufactured with ingredients that comply with FDA regulation 21 CFR 178.3570 for lubricants with incidental contact with the edible product.**H-2 Class lubricants may be used as a lubricant or anti-rust agent on equipment in which there is no possibility of the lubricated part contacting the edible product.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 99
99
Viscosity Index
150
150
ISO Grade
Saybolt Viscosity at 100°F 850 SUS
850 SUS
Saybolt Viscosity at 210°F 82 SUS
82 SUS
Kinematic Viscosity at 40°C (104°F) 164 cSt
164 cSt
Kinematic Viscosity at 100°C (212°F) 15 cSt
15 cSt
Thermal Properties Metric English Comments
Pour Point -28.9 °C
-20.0 °F
Flammability Test 565
565
[°F] Fire Point
Flash Point 246 °C
475 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 90
SAE No. 40
Users viewing this material also viewed the following: