Lotus Nano Paint NAX 01 Tow-Component Nano-paint

Category Fluid
Manufacturer Lotus Nano Paint
Trade Name NAX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotus Nano Paint NAX 01 Tow-Component Nano-paint.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: More durable and specific application methods. This paint is suitable for traffic signs on the road, cross-walks, warning vibrating lines and limited lot marking. Related machines could applied to marking lines in big amount.Applications: Urban and inter cityInformation provided by Lotus Nanopaint
Physical Properties Metric English Comments
Specific Gravity 1.60 - 1.70 g/cc
1.60 - 1.70 g/cc
ASTM D1475
Solids Content 100 %
100 %
by Weight; ASTM D1644
100 %
100 %
by Volume
Processing Properties Metric English Comments
Dry Time 0.330 hour

@Temperature 25.0 °C
0.330 hour

@Temperature 77.0 °F
ASTM D711
Descriptive Properties Value Comments
Color White, Yellow, Red and Blue
ASTM EN 1439
Curing Additive Curing
Gloss Sleek
Resin Acrylic (25-35)
Skiing Resistance (SRT) Passes (with anti-skied agent)
ASTM EN 1436
Water Resistance Passes
ASTM D870