Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lendell Medisponge®

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer Lendell Manufacturing Inc.
Trade Name Medisponge®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lendell Medisponge®.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Latex FreeThis line of foam is specifically directed towards the medical industry. This line has regulatory approval under FDA Guidelines 10993-1.Applications:Surgeons Blankets, Swabs, Wraps, Wipes, Electronic Cleanroom Wipes, Saliva Swab Kits, Industrial Scrubbers, Foam with "Super Absorbents", Enzymes in Foam, Humidor Sponges, Wicking Sponges, Foot Products, Wound Dressing, Contraceptives, Hydration Products, Medicated Foot Products, Effluent Water Filtrations, Nuclear Waste FiltrationInformation provided by Lendell Manufacturing Inc.
Physical Properties Metric English Comments
Density 0.0913 g/cc
0.00330 lb/in³
Water Absorption 17.2 %
17.2 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.170 MPa
24.6 psi
ASTM D3574
Elongation at Yield 354.7 %
354.7 %
Tear Strength 0.894 kN/m
5.10 pli
Die "C", average; ASTM D3574
2.47 kN/m
14.1 pli
Average; ASTM D3574
<= 2.52 kN/m
<= 14.4 pli
Max.; ASTM D3574
Compression Set 2.3 %
2.3 %
50%; 1H%ct
4.4 %
4.4 %
50%; 1H%cd
42.9 %
42.9 %
50%; 2E%ct
43.9 %
43.9 %
50%; 1A%ct
80.2 %
80.2 %
50%; 1A%cd
84.5 %
84.5 %
50%; 2E%cd
Descriptive Properties Value Comments
% Volume Swell 56
Saturated
CLD 50% 0.7
CLD 50% R 0.7
Comfort Factor 0.35
Expansion, % 13
in Isopropyl Alcohol
Hysteresis 14.3
IFD 25% R 22
ASTM D3574
IFD 25% RRT 18.9
ASTM D3574
IFD 65% 63.6
ASTM D3574
Recovery 85.7
Sag Factor 2.9
Water Retention, % 2.9
Wet Out, minutes 1
Users viewing this material also viewed the following: