Latrobe DuraTech™ 30 Powder Metal High Speed Steel (ASTM M3-2)

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Latrobe Steel
Trade Name DuraTech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe DuraTech™ 30 Powder Metal High Speed Steel (ASTM M3-2).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuraTech 30 super high speed steel is based upon the chemical composition of ASTM M3-2 high speed steel, but with the addition of over 8% cobalt. DuraTech 30 can be heat treated to 68 HRC. The high cobalt content enhances the attainable hardness and enables the steel to maintain high hardness at elevated service temperatures. Vanadium carbides provide the high wear resistance, and the fine grain size, small carbides, and superior cleanliness of the powder metallurgy (PM) microstructure maximize the toughness of the steel. DuraTech 30 offers improved cutting tool life compared to the M-series high speed steels, and improved toughness compared to all of the other super high speed steels, such as M42, M48, and T15. Typical applications include form tools, end mills, broaches, milling cutters, hobs, shaper cutters, taps, and any special cutting tool where high hot hardness is required.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 8.05 g/cc
8.05 g/cc
Density 8.05 g/cc
0.291 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 65.5
65.5
Oil Quenched from 1204°C, 5 minutes
66
66
Oil Quenched from 1149°C, 10 minutes
67
67
Oil Quenched from 1190°C, 5 minutes
Modulus of Elasticity 214 GPa
31000 ksi
Machinability 30 - 35 %
30 - 35 %
1% Carbon Steel
Thermal Properties Metric English Comments
CTE, linear 11.3 µm/m-°C

@Temperature 20.0 - 399 °C
6.28 µin/in-°F

@Temperature 68.0 - 750 °F
11.5 µm/m-°C

@Temperature 20.0 - 538 °C
6.39 µin/in-°F

@Temperature 68.0 - 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 1.3 %
1.3 %
Chromium, Cr 4.1 %
4.1 %
Cobalt, Co 8.25 %
8.25 %
Iron, Fe 71.2 %
71.2 %
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 5.0 %
5.0 %
Silicon, Si 0.50 %
0.50 %
Tungsten, W 6.25 %
6.25 %
Vanadium, V 3.1 %
3.1 %
Chemical Properties Metric English Comments
Critical Temperature 816 °C
1500 °F
Ac1