Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kuraray Vectran® UM 1500/300 LCP Fiber

Category Other Engineering Material , Composite Fibers , Polymer , Thermoplastic , Liquid Crystal Polymer (LCP)
Manufacturer Kuraray Company
Trade Name Vectran®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray Vectran® UM 1500/300 LCP Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
 is a high-performance multifilament yarn spun from liquid crystal polymer (LCP).  fiber exhibits exceptional strength and rigidity. Pound for pound  fiber is five times stronger than steel and ten times stronger than aluminum.  features:High strength and modulusExcellent creep resistanceHigh abrasion resistanceExcellent flex/fold characteristicsMinimal moisture absorptionHydrolytically stableResistance to organic solventsStable to acids (
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Moisture Absorption at Equilibrium <= 0.10 %
<= 0.10 %
65% RH
Loss On Ignition 30 %
30 %
Mechanical Properties Metric English Comments
Tensile Strength 3000 MPa
435000 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 103 GPa
14900 ksi
Initial Modulus
Tenacity 0.794 N/tex
9.00 g/denier
Thermal Properties Metric English Comments
Melting Point 350 °C
662 °F
Decomposition Temperature >= 450 °C
>= 842 °F
20% weight loss; TGA
Shrinkage <= 0.1 %

@Temperature 180 °C,
Time 1800 sec
<= 0.1 %

@Temperature 356 °F,
Time 0.500 hour
Hot Air
<= 0.1 %

@Temperature 100 °C,
Time 1800 sec
<= 0.1 %

@Temperature 212 °F,
Time 0.500 hour
Boiling Water
Electrical Properties Metric English Comments
Dielectric Constant <= 3

@Frequency 1e+10 Hz
<= 3

@Frequency 1e+10 Hz
Users viewing this material also viewed the following: