Material Notes:
Production Method: Obtained by interaction of stearic acid and ethylene oxide. Application: Stearox-9 is used as a spinning agent and antistatic in the production of man-made fibers.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
pH 6.0 - 9.0
6.0 - 9.0
pH of aqueous solution with 1% mass content
Component Elements Properties Metric English Comments
Free Water <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Appearance At 15°C to 25°: Pasty mass, from light-yellow to light-brown color
Saponification Number, mg of KOH/ g of Stearox-9 80-86
Users viewing this material also viewed the following: