Material Notes:
PVC Compound with addition of nitrile rubber recommended for injection of technical parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D 792
ASTM Color 25.02 - 28.02
25.02 - 28.02
Color B, ME 12
41.79 - 44.79
41.79 - 44.79
Color L, ME 12
42.59 - 45.59
42.59 - 45.59
Color A, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 43 - 47

@Time 15.0 sec
43 - 47

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 4.41 MPa
>= 640 psi
ASTM D 638
Elongation at Break >= 300 %
>= 300 %
ASTM D 638
Descriptive Properties Value Comments
Application Technical Flexible Parts
Users viewing this material also viewed the following: