Karina E 75800-35/1-B-AC Ivory PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 75800-35/1-B-AC Ivory PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.37 g/cc
1.30 - 1.37 g/cc
NBR NM-IEC 60811-1-3
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
NBR 7456
Tensile Strength >= 14.7 MPa
>= 2130 psi
NBR NM-IEC 60811-1-1
Elongation at Break >= 200 %
>= 200 %
NBR NM-IEC 60811-1-1
Electrical Properties Metric English Comments
Volume Resistivity >= 5.00e+13 ohm-cm
>= 5.00e+13 ohm-cm
NBR 5403
Descriptive Properties Value Comments
Application 75 Grades
Maximum Variation of Elongation (%) 40
NBR NM-IEC 60811-1-2
Maximum Variation of Tensile Strength (%) 30
NBR NM-IEC 60811-1-2