Karina 842-IS-SD Crystal PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 842-IS-SD Crystal PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC compound recommended for extrusion of sheet for vacuum forming (blister).Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.28 - 1.34 g/cc
1.28 - 1.34 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 24.5 MPa
>= 3560 psi
ASTM D 638
Descriptive Properties Value Comments
Application Blister
Clarity OK
ME 03