KKPC KOSYN KSL 362 Styrene-Butadiene Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Korea Kumho Petrochemical Co., Ltd.
Trade Name KOSYN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KKPC KOSYN KSL 362 Styrene-Butadiene Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-Butadiene LatexCharacteristics: KOSYN KSL 300 series is a Styrene-Butadiene Latex. KSL 362 is a styrene-butadiene latex for cement mortar. Because it has good miscibility with cement, its addition to concrete elevates waterproofing, impact-resistance, and reinforcement. Applications: Oil-resistant Foam Rubber, For Impregnation of Tire and Belt Cord, Foam Backing of Textile Goods, Coating of Textile, Foam Rubber, Base Latex of ABS resin, Deck Covering of Ship, Reinforcement of Bridge, Waterproofing, Cement Mortar, Reinforcing agent of Foam ProductsThis product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.Data provided by Korea Kumho Petrochemical Co., Ltd.
Physical Properties Metric English Comments
Solids Content 48.5 %
48.5 %
pH 10
10
at 25°C
Viscosity 80 cP
80 cP