Johnson Matthey SC 900 Platinum w/ 10% Palladium Jewelry Alloy

Category Metal , Nonferrous Metal , Precious Metal , Platinum Alloy
Manufacturer Johnson Matthey
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey SC 900 Platinum w/ 10% Palladium Jewelry Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose. Palladium has been used to create casting alloys at various levels of fineness. Palladium produces a softer casting.
Physical Properties Metric English Comments
Density 19.8 g/cc
0.715 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 72
72
As Cast
80
80
Annealed
Elongation at Break 22 %
22 %
Annealed
22 %
22 %
As Cast
Thermal Properties Metric English Comments
Melting Point 1740 - 1755 °C
3160 - 3191 °F
Solidus 1740 °C
3160 °F
Liquidus 1755 °C
3191 °F
Component Elements Properties Metric English Comments
Palladium, Pd 10 %
10 %
Platinum, Pt 90 %
90 %