Johnson Matthey JM Tenacity 2 Brazing Flux Powder

Category Metal , Nonferrous Metal , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey JM Tenacity 2 Brazing Flux Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
JM Tenacity No 2 flux is highly active with a working range up to 1480°F. It can be used on most metals, except for Aluminum and magnesium, for brazing with silver brazing alloys. JM Tenacity No 2 flux powder can be used to braze stainless steel provided that brazing temperature is below 1300°F. JM Tenacity No 2 powder is ideal for hot rodding or application as a water-based paste. Flux residues can be removed with hot water after brazing. Residues: Water solubleInformation provided by Johnson Matthey.
Thermal Properties Metric English Comments
Active Range 550 - 800 °C
1020 - 1470 °F