Intercontinental Polymers HoPET 741-01 HoPET Polymer Type - Semi-Dull, Polyester Pellets

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Intercontinental Polymers, Inc.
Trade Name HoPET
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Intercontinental Polymers HoPET 741-01 HoPET Polymer Type - Semi-Dull, Polyester Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Filament Yarn Information provided by Intercontinental Polymers.
Physical Properties Metric English Comments
Viscosity Measurement 0.63 - 0.65
0.63 - 0.65
Intrinsic; LCL-PR21
Optical Properties Metric English Comments
Gardner Color Number 2.7 - 4.7
2.7 - 4.7
+ b; LCL-PR01
65 - 75
65 - 75
Rd; LCL-PR01
Processing Properties Metric English Comments
Melt Temperature 255 °C
491 °F
LCL-PR29
Moisture Content <= 0.25 %
<= 0.25 %
LCL-PR08
Descriptive Properties Value Comments
COOH Max 45 meq/kg
LCL-PR09
DEG 0.7 - 0.9 wt%
LCL-PR11
TiO2 0.33 - 0.37 wt%
LCL-PR02