Intercontinental Polymers HoPET 720 HoPET Polymer Type - Film Grade Resin, Clear, Polyester Pellets

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Intercontinental Polymers, Inc.
Trade Name HoPET
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Intercontinental Polymers HoPET 720 HoPET Polymer Type - Film Grade Resin, Clear, Polyester Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: FilmInformation provided by Intercontinental Polymers.
Physical Properties Metric English Comments
Viscosity Measurement 0.575 - 0.605
0.575 - 0.605
Intrinsic; LCL-PR21
Ash <= 0.050 %
<= 0.050 %
LCL-PR36
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Gardner Color Number 4.0 - 7.0
4.0 - 7.0
+ b; LCL-PR01
70 - 80
70 - 80
Rd; LCL-PR01
Electrical Properties Metric English Comments
Electrical Resistivity <= 5.00e+6 ohm-cm
<= 5.00e+6 ohm-cm
Processing Properties Metric English Comments
Melt Temperature 255 °C
491 °F
LCL-PR29
Moisture Content <= 0.25 %
<= 0.25 %
LCL-PR08
Descriptive Properties Value Comments
COOH 18 - 38 meq/kg
LCL-PR09
DEG 0.65 - 0.95 wt%
LCL-PR11