Intercontinental Polymers HoPBN 312 HoPBN Polymer Type - Clear, Polyester Pellets

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Intercontinental Polymers, Inc.
Trade Name HoPBN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Intercontinental Polymers HoPBN 312 HoPBN Polymer Type - Clear, Polyester Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Intercontinental Polymers.
Physical Properties Metric English Comments
Viscosity Measurement 0.65 - 0.71
0.65 - 0.71
Intrinsic; LCL-PR21
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Gardner Color Number 2.5 - 7.5
2.5 - 7.5
+ b; LCL-PR01
73 - 93
73 - 93
Rd; LCL-PR01
Processing Properties Metric English Comments
Melt Temperature 240 °C
464 °F
LCL-PR29
Descriptive Properties Value Comments
COOH 15 - 75 meq/kg
LCL-PR09