Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos T00G-00 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos T00G-00 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a fractional MFR polypropylene impact copolymer designed for the roofing membrane market. Its blend of impact resistance and flexural modulus is designed to provide an excellent balance between processing and performance. This meets FDA requirements of 21CFR 177.150(c), 3.4.ApplicationsReinforced Roofing membraneBenefitsGood toughnessFlexibilityGood MD and TD tear strengthGood and consistent processabilityWind resistanceGood weldabilityInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
Instantaneous; ASTM D2240
Tensile Strength, Yield 8.96 MPa

@Temperature 23.0 °C
1300 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Flexural Modulus, 1% Secant 172 MPa

@Temperature 23.0 °C
25000 psi

@Temperature 73.4 °F
0.05 in/min test speed
Izod Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256