Indorama AlphaPet Preformance® 1708HS(A) PET Resin

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Indorama AlphaPet
Trade Name Preformance®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indorama AlphaPet Preformance® 1708HS(A) PET Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Preformance® PET 1708HS(A) is a food grade PET copolymer that is suitable for a wide variety of beverage and juice containers hot fill application, high temperature filling. Offers exceptional clarity and color and is engineered for heat-set. The low acetaldehyde content in the resin helps eliminate any impact on aroma and flavor. Preformance® PET 1708HS(A) resin is considered safe for food packaging applications based upon compliance with FDA Regulation 21 CFR Section 177.1630 specifications.
Physical Properties Metric English Comments
Bulk Density 0.817 - 0.881 g/cc
0.0295 - 0.0318 lb/in³
QCL-03-0004
Viscosity Measurement 0.78 - 0.82
0.78 - 0.82
[dl/g], Intrinsic; QCL-03-0015
Chemical Properties Metric English Comments
Acetaldehyde <= 2.00 ppm
<= 2.00 ppm
QCL-03-0001
Processing Properties Metric English Comments
Moisture Content <= 0.25 %
<= 0.25 %
as packed, QCK-03-0011
Descriptive Properties Value Comments
Color, CIE > 78 (L)
QCL-03-0009
-4.0 to 1.0 (b)
QCL-03-0009
Contaminants/Black Specs None
QCL-03-0028
Dust <300 ppm
as packed, QCL-03-0014
Process Blow Molding
Injection Molding
Region US & Canada
Bamberger Polymers Distribution