Material Notes:
Weight per Epoxide (EEW, g/eq) 1666 to 2000. Max color is 4.Comments/Applications: GT 7097 - 55% solids in MIBK (22.5%) and toluene (22.5%). For heat cured industrial coatings in combination with urea, melamine and/or phenolic resins. Viscosity, Gardner Holdt at 25°C: Y-Z2Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 1800 - 4500 cP
1800 - 4500 cP