Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® EH04 Epoxy Resin System, T600 Fiber

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® EH04 Epoxy Resin System, T600 Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
T24K 150 24" EH04 36%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2270 MPa
329000 psi
Tensile Modulus 118 GPa
17100 ksi
Flexural Yield Strength 1480 MPa
214000 psi
Flexural Modulus 114 GPa
16500 ksi
Compressive Yield Strength 1650 MPa
240000 psi
Compressive Modulus 123 GPa
17800 ksi
Shear Strength 88.9 MPa
12900 psi
Short Beam
Users viewing this material also viewed the following: