Material Notes:
Turco 6871 is a new environmentally sustainable cleaner that is low VOC, and free of chromates, phosphates and silicates. This alkaline cleaner is dilutable with water to clean painted and unpainted exterior aircraft surfaces by spraying or foaming methods. MIL-DTL-8777D and MIL-DTL-87937 approved.Application: Aircraft Appearance
Descriptive Properties Value Comments
Chemistry Alkaline, Water-based
Consistency Liquid
Form Concentrated