Henkel Alodine 5700 Wipes Conversion Coating, Touch Up

Category Fluid , Solvent
Manufacturer Henkel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Alodine 5700 Wipes Conversion Coating, Touch Up.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alodine 5700 Wipes are a chromium-free conversion coating specifically formulated for treating aluminum and its alloys. This product is formulated as a Ready-to-Use material for wipe applications. The process provides an excellent base for organic finishes.
Descriptive Properties Value Comments
Chemistry Non-chrome
Consistency Liquid
Form Presaturated Wipe
Substrate Aluminum