Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

H.C. Starck Amperit® 849.054 Sintered Yttria (Y2O3)

Category Ceramic , Oxide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 849.054 Sintered Yttria (Y2O3).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Particle Size 10 µm
10 µm
Maximum of 5% less than
15 µm
15 µm
Maximum of 15% less than
45 µm
45 µm
Maximum of 5% greater than
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.020 %
<= 0.020 %
Calcium, Ca <= 0.020 %
<= 0.020 %
Carbon, C <= 0.10 %
<= 0.10 %
Iron, Fe <= 0.050 %
<= 0.050 %
Molybdenum, Mo <= 0.010 %
<= 0.010 %
Silicon, Si <= 0.10 %
<= 0.10 %
Y2O3 99.6 - 100 %
99.6 - 100 %
Zirconium, Zr <= 0.10 %
<= 0.10 %
Users viewing this material also viewed the following: