Material Notes:
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance properties. These products can be injection molded, blow molded, and extruded. These are used for biomedical and drug administration applications.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength 31.0 MPa
4500 psi
ASTM D412
Tensile Strength, Yield 2.30 MPa

@Strain 50.0 %
334 psi

@Strain 50.0 %
ASTM D412
3.20 MPa

@Strain 100 %
464 psi

@Strain 100 %
ASTM D412
5.90 MPa

@Strain 300 %
856 psi

@Strain 300 %
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412
Tear Strength 400 kN/m
2280 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 5.0
5.0
ASTM D1044(Taber) H-22
Compression Set 25 %

@Temperature 23.0 °C,
Time 79200 sec
25 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
35 %

@Temperature 70.0 °C,
Time 79200 sec
35 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Copyright © lookpolymers.com All Rights Reserved