ExxonMobil Vistalon™ 8700 Bimodal EPDM Polymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Exxon Chemical
Trade Name Vistalon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Vistalon™ 8700 Bimodal EPDM Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vistalon 8700 EPDM rubber is a grade of high molecular weight with a low ethylene content and a high diene level. It is produced with ExxonMobil Chemical's proprietary technology offering bimodal molecular weight distribution (MWD). This grade is ideal for the manufacture of extruded profiles combining good green strength and smooth extrusion.Key Features: Designed for: Constant quality of mixed compound.Improved productivity of mixing and sponge extrusion.Reduced inventories by using a single grade. Good green strength. Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Mooney Viscosity 78

@Temperature 125 °C
78

@Temperature 257 °F
ML 1 + 4; ASTM D1646
Descriptive Properties Value Comments
ENB Content 8%
ASMT D6047
Ethylene Content 63%
ASTM D3900