ExxonMobil Vistalon™ 6602 Ethylene Propylene Diene Terpolymer Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Exxon Chemical
Trade Name Vistalon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Vistalon™ 6602 Ethylene Propylene Diene Terpolymer Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Vistalon 6602 EPDM rubber is a medium ENB polymer with low ethylene and medium-high Mooney. It has broad molecular weight distribution for excellent compounding processibility. It is applicable for extruded applications like automotive weatherseals or hoses, combining high collapse resistance and smooth extrusion. It may also be used in molded applications requiring good compression set.Key Features:Excellent processibility resulting in shorter mixing and molding times.Good low temperature properties.Good low temperature flexibility and compression set.High collapse resistance.Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Mooney Viscosity 80

@Temperature 125 °C
80

@Temperature 257 °F
ML(1+4), Radial cavity dies, polymer remassed at 145±°C; ASTM D1646
Descriptive Properties Value Comments
Ethylene Content 55 %
ASTM D3900
Ethylidenenorbornene (ENB) Content 5.2%
ASTM D6047