ExxonMobil Santoprene® 8191-60B500 Thermoplastic Vulcanizate  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8191-60B500 Thermoplastic Vulcanizate  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA 6, PA 6/6, PA 6 GF, PA 11, PA 12 and PA 6/12 substrates in applications where hard/soft combinations are required. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Key Features:Designed for excellent adhesion to PA6, PA6/6, PA6GF, PA11, PA 12 and PA6/12 (cold insert or 2K [two-shot] molding).Broad processing window for injection molding.Recommended for applications requiring superior part surface appearance.EU and China RoHS compliant.Information provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 65

@Time 15.0 sec
65

@Time 0.00417 hour
2 mm; ISO 868
Tensile Strength at Break 2.80 MPa
406 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 2.10 MPa

@Strain 100 %
305 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 200 %
200 %
Across Flow; ASTM D412 and ISO 37
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.10 mm
HB

@Thickness 0.0433 in
UL File Number - E80017
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in