ExxonMobil SAE 40 Mobilgard ADL Series

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil SAE 40 Mobilgard ADL Series.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobilgard ADL Series by ExxonMobil is a high performance family of increased dispersancy engine oils for high BMEP medium and high-speed diesel engines operating on distillate and MDO fuels. These advanced diesel lubricants are available in both SAE 30 and 40 grades to suit most marine engine viscosity requirements. As a result of a special balance of detergent and dispersant properties these oils provide not only increased resistance to cylinder liner lacquer formation in severe service applications, but also assist in sludge and deposit removal. Use of Mobilgard ADL Series oils avoids high oil consumption associated with cylinder liner lacquering, improves overall engine cleanliness and can increase time between engine overhauls. Superior load carrying properties minimise piston ring and liner wear, and also make Mobilgard ADL Series lubricants suitable for marine gearing applications.Mobilgard ADL Series lubricants are intended for use in high BMEP engines and in severe duty engine applications where the nature of the fuel and service requires a greater level of detergency/dispersancy and liner lacquer control than is offered by most diesel engine lubricants. These lubricants also have high FZG ratings, which makes them excellent extreme pressure gear lubricants.
Physical Properties Metric English Comments
Specific Gravity 0.901 g/cc
0.901 g/cc
15°C
Viscosity Measurement 101
101
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 141 cSt
141 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 14.5 cSt
14.5 cSt
ASTM D445
Ash 2.3 %
2.3 %
Sulfated Ash, wt%; ASTM D874
Thermal Properties Metric English Comments
Pour Point -9.00 °C
15.8 °F
ASTM D97
Flash Point 244 °C
471 °F
ASTM D92
Chemical Properties Metric English Comments
Total Base Number 15
15
mgKOH/g; ASTM D2896
Descriptive Properties Value Comments
FZG 4-Square Load Support, DIN 51354, Fail Stage 12