ExxonMobil PP2252E4 Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP2252E4 Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Medium melt flow rate homopolymer designed for high speed extrusion of woven fabrics exhibiting low water carry over.Availability: North America and South America Features:Balanced Stiffness/ToughnessGeneral PurposeLow Water CarryoverUses: Carpet BackingCompoundingFabricsFibersPackagingProcessing Method: ExtrusionInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 4.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238