Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Label-Lyte® 150 LL-302 White Opaque OPP Facestock

Category Polymer , Adhesive , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte® 150 LL-302 White Opaque OPP Facestock.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
White, corona-treated polypropylene label facestock designed for rigid and semi-rigid pressure-sensitive applications requiring durability, opacity, and excellent graphic appeal. The treated, high energy, print surface has generally good compatibility with water-based and solvent-based flexo and gravure, UV flexo, UV letterpress, and UV screen ink systems. The print surface is also compatible with hot stamping systems. The adhesive side is corona-treated for good pressure-sensitive adhesive anchorage.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Thickness 66.0 microns
2.60 mil
Coating Weight >= 46.1 g/m²
>= 28.8 lb/ream
520
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 200 %
200 %
510
Film Elongation at Break, TD 50 %
50 %
510
Film Tensile Strength at Break, MD 90.163 MPa
13077 psi
510
Film Tensile Strength at Break, TD 190.93 MPa
27692 psi
510
Thermal Properties Metric English Comments
Shrinkage, MD 5.0 %
5.0 %
at 275°F; 438
Shrinkage, TD 5.0 %
5.0 %
at 275°F; 438
Optical Properties Metric English Comments
Gloss 70 %
70 %
442
Transmission, Visible 19 %
19 %
417
Descriptive Properties Value Comments
Gurley Stiffness, MD, mgf 22
Gurley Stiffness, TD, mgf 42
Wetting Tension, receding COS theta .85 adhesive surface
0.9
print surface
Yield, in2/lb 15000
Users viewing this material also viewed the following: