ExxonMobil Jayflex™ DIDP Plasticizer (Asian Grade)

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Exxon Chemical
Trade Name Jayflex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Jayflex™ DIDP Plasticizer (Asian Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Asia PacificCAS Number: 68515-49-1Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.962 - 0.971 g/cc
0.0348 - 0.0351 lb/in³
ASTM D4052
Maximum Moisture Content 0.10
0.10
ASTM E1064
Chemical Properties Metric English Comments
Acid Value <= 0.010
<= 0.010
[mg KOH/g]; ASTM D1045
Descriptive Properties Value Comments
Color <30 Pt-Co
ASTM D1209
Ester Content >99.6%
RPP 201