ExxonMobil Greasrex K-170

Category Fluid , Lubricant , Lithium Gellant
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Greasrex K-170.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greasrex K-170 is a high performance lithium hydroxystearate grease, formulated especially to resist oil separation in high speed rotating equipment, to protect against wear, and to provide protection against rust and corrosion. Greasrex K-170 is a multi-purpose grease designed for use in high speed rotating equipment, such as electric drills.Greasrex K-170 is recommended for all types of applications where high rotational speeds are encountered.  In particular, it: provides good low temperature pumpability and is suitable for centralized lubrication systems and other applications where low temperature performance is required; is recommended for multipurpose applications in antifriction and plain bearings, bushings and pins under normal operating conditions; is recommended for lubrication of electric hand tools, where high speeds, and moderately loaded bearings are found
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 24 cSt
24 cSt
ASTM D445
Mechanical Properties Metric English Comments
Penetration 300
300
Worked, 25°C; ASTM D217
Timken Test 18100 g
40.0 lb
Thermal Properties Metric English Comments
Dropping Point 175 °C
347 °F
ASTM D2265
Descriptive Properties Value Comments
Color light brown
Corrosion Prevention, ASTM D1743 pass
Soap/Thickener Type lithium