Esstech X-942-7244 Ethyleneglycol Dimethacrylate, C10H14O4

Category Polymer , Thermoset , Methacrylate
Manufacturer Esstech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-942-7244 Ethyleneglycol Dimethacrylate, C10H14O4.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ethyleneglycol dimethacrylate, EGDMA acts as a cross-linking agent between polymer chains. Also known as ethylene dimethacrylate or monoethylene glycol dimethacrylate, this difunctional monomer has similar reactivity to methyl methacrylate and low water absorptivity. Listed on the Toxic Substance Control Act List. CAS # 97-90-5.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Molecular Weight 198.218 g/mol
198.218 g/mol
Optical Properties Metric English Comments
Refractive Index 1.453
1.453
Processing Properties Metric English Comments
Moisture Content <= 0.25 %
<= 0.25 %
Descriptive Properties Value Comments
Acidity (% Methacrylic Acid) < 0.01
Color (APHA) < 10
MeHQ Inhibitor (ppm) 40-80
Purity (%) > 99