Eastman Eastman F-Cat HC Polyester Concentrate

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Eastman
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastman F-Cat HC Polyester Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Carpet FibersProduct Description: Eastman Polymer F-Cat HC is a polyester concentrate intended to impart cationic dyeable properties to extruded polyester fibers. The primary application is a polyester BCF yarns intended for griege goods dyeing. The addition of Eastman Polymer F-Cat HC to extruded yarn supports interest in producing a multi-tonal carpet, that can be griege goods dyed to greatly differing colors when a finished carpet is produced from both traditional and cationic infused yarns. By varying the levels of concentration of Eastman Polymer F-Cat HC in the yarns, it would also be possible to produce different degrees of cationic colored goods.Information provided by Eastman.
Physical Properties Metric English Comments
Bulk Density 0.827 g/cc
0.0299 lb/in³
Viscosity Measurement 0.26 - 0.32
0.26 - 0.32
dL/g; Inherent; EMN-A-AC-G-V-1
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 45.0 - 48.0 °C
113 - 118 °F
Dry Polymer
Descriptive Properties Value Comments
Color Pale Amber
Form Pellets