Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ELM® NSF H1 Food Grade Chain and Cable Lubricant

Category Fluid , Lubricant
Manufacturer ELM®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELM® NSF H1 Food Grade Chain and Cable Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ELM Chain Lubricant – Food Grade is a high performance food grade chain lubricant formulated with the best optimized USA-grown natural seed oils and select additives, it surpasses the lubricity and performance of conventional chain lubricants. It is NSF (National Sanitary Foundation) approved H1 for incidental food contact. NSF Registration No. 142552Applications: General purpose chain lubricantUse for chains, cables, rollersNSF H1 Approved for incidental food contactBenefits: Reduces product inventorySuperior lubricity improves productivityLess mist generationSafe for all metalsWill help your business comply with ISO-14000Does not contain chlorineHigh flash and fire pointsMade from renewable USA-grown crop-based vegetable oilsInformation provided by ELM®
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 44 cSt
44 cSt
ASTM D445
Thermal Properties Metric English Comments
Flash Point 306 °C
583 °F
ASTM D92
Descriptive Properties Value Comments
Appearance Light Yellow
Fire point 324°C
ASTM D92
Users viewing this material also viewed the following: