Material Notes:
Calprene 487 is a 45/55 Butadiene/Styrene thermoplastic copolymer, polymerized in solution. It has a radial structure and is extended with 40 phr of paraffinic oil.This product is presented in pellet form and has very adequate flow properties for compounding articles intended for injection.Applications:FootwearSportswearMechanical rubber goodsInformation provided by Dynasol
Physical Properties Metric English Comments
Volatiles <= 0.40 %
<= 0.40 %
ASTM D-5668
Melt Flow 14 g/10 min

@Load 5.00 kg,
Temperature 190 °C
14 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D-1238
Ash <= 0.35 %
<= 0.35 %
ASTM D-5667
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
ASTM D-2240
Abrasion 140
140
mm³; DIN 53516
Chemical Properties Metric English Comments
Styrene Content 55 %
55 %
on polymer; ASTM D-5775
Descriptive Properties Value Comments
Hunterlab color, max 2
Insolubles in toluene, 325 mesh, % max 0.1
Oil Content, % 28.5
ASTM D-5774