Dyna-Purge® M Purging Compound

Category Polymer , Thermoplastic , Purging Compound
Manufacturer Shuman Dyna-Purge®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dyna-Purge® M Purging Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Most versatile & widely used in the Plastics IndustryGeneral Description:DYNA-PURGE M is a versatile non-abrasive, non-chemical “engineered” thermoplastic purging compound, formulated to flow naturally through the barrel and hot runner system of the injection molding machine, as well as extrusion equipment. A non-melting but softening thermoplastic scrubs the screw and barrel, while the carrier matrix flushes away impurities.FEATURES & BENEFITS OF DYNA-PURGE MDeveloped for color changes, resin changes, preventative machine maintenance and before manual cleaningExcellent for purging through hot runner systems with a minimum clearance of .030 inch (.75 mm)Effective through a wide temperature range 350°F to 600°F(177°C to 315°C)Easy to use – no process adjustment necessary – use at the resident resin processing temperature and RPM speedNon-abrasive, non-melting but softening thermoplastic, which thoroughly loosens carbonized and degraded resin, allowing it to be flushed out of the systemSafe, non-hazardous, with no chemicals – ingredients are FDA compliantHeat stable – recommended during shutdown and start-upLow “cost-per-purge” – only small quantity needed to be effectiveNo mixing required – simply use “as is”Unlimited shelf life
Processing Properties Metric English Comments
Processing Temperature 177 - 315 °C
351 - 599 °F
Injection
177 - 315 °C
351 - 599 °F
Extrusion
Descriptive Properties Value Comments
Amount of Purge (Extrusion) Approx. 10 lbs per diameter inch of screw
L:D dependant
Amount of Purge (Injection) Approx. 2 lbs per diameter inch of screw
Minimum Orifice (Extrusion) .03in, .75mm
Die
Minimum Orifice (Injection) .03in, .75mm
Nozzle
Screen Packs or other flow restrictions (Ext.) Must be removed (otherwise use Dyna-Purge X,SF or F)
Screen Packs or other flow restrictions (Inj.) Must have minimum clearance of .03in (.75mm)
Types of Resins All