Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 539 Polyester Film, 370 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 539 Polyester Film, 370 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 539 is a two sided treated grade of clear film for applications where freedom from static is required. Its main use is as a montage "foil" in the production of printing plates. Melinex® 539 is available in thicknesses of 370, 500 and 700 gauge. Melinex® 539 is supplied as a knurled reel but is readily available in unknurled reel sheet form through a quality and stockists and distributors worldwide where it is usually referred to as Melinex® 538.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 171 MPa
24800 psi
ASTM D882A
Film Tensile Strength at Break, TD 171 MPa
24800 psi
ASTM D882A
Thermal Properties Metric English Comments
Melting Point 255 - 260 °C
491 - 500 °F
ASTM E794-85
Shrinkage, MD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze <= 1.5 %
<= 1.5 %
ASTM D1003
Transmission, Visible 88 %
88 %
TLT; ASTM D1003
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+10 ohm

@Temperature 20.0 °C
1.00e+10 ohm

@Temperature 68.0 °F
500 V DC @ 60% RH; ASTM D257
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved