Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Kalrez® Spectrum™ 6380 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Kalrez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Kalrez® Spectrum™ 6380 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Kalrez® Spectrum™ 6380 perfluoroelastomers parts are a non-black product specifically developed for chemical processes involving hot, aggressive amines. In addition, it has excellent overall chemical resistance (see chart below). This cream colored product is easily identifiable when selecting an O-ring material for harsh chemical plant services. This material has excellent mechanical properties and is a top choice for both static and dynamic sealing applications. A maximum continuous service temperature of 225 °C is suggested while short-term excursions to higher temperatures are permissible.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength at Break 15.86 MPa
2300 psi
ASTM D412
Elongation at Break 160 %
160 %
ASTM D412
100% Modulus 0.00689 GPa
0.999 ksi
ASTM D412
Compression Set 40 %

@Temperature 204 °C,
Time 252000 sec
40 %

@Temperature 399 °F,
Time 70.0 hour
ASTM D395B
Descriptive Properties Value Comments
Color Cream