70 Durometer, 2-part, 1 to 1 mix, oil resistant, tan Liquid Silicone Rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc

@Temperature 25.0 °C
1.46 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength, Ultimate 6.58 MPa
954 psi
Elongation at Break 255 %
255 %
Tear Strength 17.5 kN/m
100 pli
Compression Set 33.5 %
33.5 %
Descriptive Properties Value Comments
Color tan