Dow Corning SILASTIC® L RTV SILICONE RUBBER BASE & CURING AGENT

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® L RTV SILICONE RUBBER BASE & CURING AGENT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low durometer silicone mold making rubber recommended for use with rigid polyurethanes and can be used with polyesters and epoxies.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc

@Temperature 25.0 °C
1.27 g/cc

@Temperature 77.0 °F
Viscosity 100000 cP
100000 cP
mixing, dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 34
34
Tensile Strength, Ultimate 3.79 MPa
550 psi
Elongation at Break 350 %
350 %
Tear Strength 8.77 kN/m
50.0 pli
Descriptive Properties Value Comments
Color green
Mix Ratio (X:1) 10
Base to Catalyst
Working Time (min) 60