Dow Corning FOX® PMCP13 Flowable Oxide

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name FOX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning FOX® PMCP13 Flowable Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Spin-on dielectric (HSQ)Information provided by Dow Corning
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Film density
Thickness 0.174 - 0.333 microns
0.00685 - 0.0131 mil
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Electrical Properties Metric English Comments
Dielectric Constant 2.9

@Frequency 1.00e+6 Hz
2.9

@Frequency 1.00e+6 Hz
Descriptive Properties Value Comments
Film Non-Uniformity (max % RSD) 1