Polymer Property : Film Tensile Strength at Break, MD = 100 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Dow Corning FOX® PMCP12 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Dow Corning FOX® PMCP13 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Dow Corning FOX® PMCP14 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Dow Corning FOX® PMCP15 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Dow Corning FOX® PMCP16 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Dow Corning FOX® PMCP17 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Dow Corning FOX® PMCP22 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Dow Corning FOX® PMCP23 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Dow Corning FOX® PMCP24 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Dow Corning FOX® PMCP25 Flowable Oxide
Spin-on dielectric (HSQ)Information provided by Dow Corning
Film Tensile Strength at Break, MD 80.0 - 100 MPa
11600 - 14500 psi
Average value: 88.0 MPa Grade Count:22
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..