Material Notes:
Silicone polyether, acts as a performance booster for crude oil emulsion breakers.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity Measure 425 cSt
425 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point 60.0 °C
140 °F
Closed cup
Processing Properties Metric English Comments
Shelf Life 30.0 Month
30.0 Month
Descriptive Properties Value Comments
HLB Ratio (%) 14
Non-Ionic Yes
Water Soluble Yes