Dow Corning 92-023 PRIMER

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 92-023 PRIMER.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.720 g/cc
0.720 g/cc
Volatiles 93 %
93 %
Viscosity 0.70 cP
0.70 cP
dynamic
Thermal Properties Metric English Comments
Flash Point -4.00 °C
24.8 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Appearance clear liquid
Hydrophobic yes
Solvent heptane
Water Resistant yes