Dow Corning 670 Fluid

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 670 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A blend of approximately 50 percent cyclopentasiloxane and approximately 50 percent polypropylsilsesquioxane, especially useful in color cosmetic formulations.Information provided by Dow Corning
Physical Properties Metric English Comments
Solids Content 50 %
50 %
Viscosity Measure 200 cSt
200 cSt
Optical Properties Metric English Comments
Refractive Index 1.4197
1.4197
Descriptive Properties Value Comments
Cyclotetrasiloxane Content (%) <1