Covestro Desmopan® DP 8795 A Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 8795 A Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
injection molding gradewith special UV stabilizersEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
3s; ISO 868
Hardness, Shore D 41
41
15s; ISO 868
Abrasion 26
26
mm³; ISO 4649
Compression Set 20 %

@Temperature 23.0 °C
20 %

@Temperature 73.4 °F
ISO 815
40 %

@Temperature 70.0 °C
40 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America