Material Notes:
Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosive acids from the pickling solution contaminate the oil supply. The oil neutralizes these common acids before they can etch the bearing journals and pads. This is especially valuable during shutdown periods. Bearing Oil extends bearing life and reduces the downtime required for bearing changeouts for the roll stands. Bearing Oil is available in ISO grade 460. Bearing oil exceeds the requirements of the Morgoil Lubricant Specification for use in roll-neck bearings.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Specific Gravity 0.884 g/cc
0.884 g/cc
60°F
API Gravity 28.6 °
28.6 °
Viscosity Measurement >= 98
>= 98
Viscosity Index; ASTM D 2270
Kinematic Viscosity at 40°C (104°F) 219 cSt
219 cSt
Kinematic Viscosity at 100°C (212°F) 19.1 cSt
19.1 cSt
ASTM Color 4.0
4.0
ASTM D 1500
Thermal Properties Metric English Comments
Pour Point <= -9.44 °C
<= 15.0 °F
ASTM D 97
Flash Point >= 282 °C
>= 540 °F
ASTM D 92
Chemical Properties Metric English Comments
Total Acid Number 0.80
0.80
ASTM D974
Descriptive Properties Value Comments
Copper Strip Max 1A
ASTM D130
Emulsion Max 0.5 ml
Emulsion Characteristics (40-38-2) 15 minutes
ASTM D-1401, 180°F
Foam Characteristics Sequence I Max 0-0-0
ASTM D892
Free Water From Centrifuge 1 ml
Free Water From Sep Funnel 32.5 ml
ASTM D4172
Rust (Part B) Pass
ASTM D655
Total Free Water Min 33.5 ml
Water in Oil Max 0.5 %